This is a picture of my first efort at the Moreau method of making a glass blank from slumped plate glass, the first two layers are 3/8" thick and all others are 1/4" (they all should have been 3/8") the back is flat and the front is a pregenerated F4 curve (the defective surface on the face was due to an error in mold prep). I have not yet tested it for residual strain but feel confident it can be worked with. I think this methoud may hold promise. Thanks to Jean-Guy Moreau and evreyone else for your help.
Attached Image: