I getting ready to make a pitch lap for a 12.5 inch mirror.
I have some pitch from a batch made for ATM use several years ago. The label says Gugulz (made in Switzerland) and looks like pitch alright. It's #73.
I read somewhere that one should add a bit of turpentine before heating.
Can I use "white spirit" paint thinner? (I have industrial quantities of that stuff lying around.)
Can I use mineral turpentine? (Dirt cheap and available.)
In Kenya (where I live) nobody sells wood turpentine.
Clears,
Joe
I have some pitch from a batch made for ATM use several years ago. The label says Gugulz (made in Switzerland) and looks like pitch alright. It's #73.
I read somewhere that one should add a bit of turpentine before heating.
Can I use "white spirit" paint thinner? (I have industrial quantities of that stuff lying around.)
Can I use mineral turpentine? (Dirt cheap and available.)
In Kenya (where I live) nobody sells wood turpentine.
Clears,
Joe
In lumine tuo videbimus lumen.
8O Home-made 10” Dob / Home-made 4” refractor
EPs: Konig 32mm (1.25") / Zhumell WF 30mm (2") / Nagler 13mm T1 / Orion Sirius Plossls 25 & 10mm / Zhumell Plossl 9 mm / Meade MA 9mm