i have just recently started hypering my own techpan film. the first roll, i hypered at 90hrs, +3psi @ 50deg C. I processed it at 16min in HC110 delution B. It is a rather dark negative. Does anyone have a suggestion on developing time for hypered Tech Pan film in HC110 delution B? What developing time for non-hypered film? My latest roll of film i am trying the hypering at 17hrs, +18psi @ 50deg C. Would this make for a different developing time? Also i notice alot of people use D-19 developer for hypered Techpan, what advantage does it give me over the HC110? Any comments would be appreciated.
Thanks
Thanks